Back in the 70's Wurlitizer used to reccomend a mixture of 7 to 1 naptha & mineral oil as a flange lube. Messy, but it worked. -----Original Message----- >From: Avery <avery1 at houston.rr.com> >Sent: Apr 8, 2006 2:03 PM >To: joegarrett at earthlink.net, Pianotech List <pianotech at ptg.org> >Subject: Re: Correction!...was Lubricating Sting Bearing Points > >Joe, > >I'm talking about before Silicone!!!! :-) > >Avery > >At 01:28 PM 4/8/2006, you wrote: > >>Yikes! The Brain Cells, (or lack thereof), failed me again. The Mix >>that Wurlizter used was Silicone and NAPTHA! Sorry about >>that!????<G> Damned stuff goes where you don't want it. DAMHIK! >> >> >>Joe Garrett, R.P.T. (Oregon) >>Captain, Tool Police >>Squares R I >> >> >
This PTG archive page provided courtesy of Moy Piano Service, LLC